calibrating resin and anti-aliasing settings
Anti-aliasing is generally unnecessary on modern high-resolution resin printers, while proper exposure and lift calibration minimize visible layer lines.
- Anti-aliasing and blur settings are located in Lychee's Export tab, but are largely redundant on modern high-resolution screens and reduce screen lifespan
- For a 35 micron pixel size, matching layer height to 35 microns is advised, testing with and without anti-aliasing to compare quality
- Layer lines caused by fresh PFA film or uncalibrated resin can be fixed by lowering lift speed, slightly increasing lift distance, and tuning exposure time
- For ABS-like resin at 30 micron layers, 25 seconds of bottom exposure may risk poor bed adhesion depending on the build plate
- Calibration prints printed directly on the build plate require checking specific test guidelines to ensure over-exposed bottom layers do not distort results